You can treat it as an Section VIII Appendix II Flange. Hopefully the two stud bolts that you cannot insert, are 180° apart.


On Tue, Apr 28, 2009 at 1:21 AM, ptvvtp <cezond31@gmail.com> wrote:

 We have the following  scenario in one of our projects . Due to
inadequate space availability caused by the valve body studs, the
piping flange studs could not be inserted into the flange joint.. The
case in question is a 10" , 900# Flange which carries 16 no.s studs.
It is not possible to insert 2no.s stud bolts in the flange joint.
Does B16.5 mention anything about the safety / operability / validity
of a flange joint which has two no.s stud bolts less in a 16 stud
flange joint ?




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...