The base material is not a problem. The problem is:
1. Filler material is one of essential variable.
2. impact test it's requiered low design temperature.
 
For A333 I use ER80S Ni1 filler material.

--- On Thu, 4/23/09, Endri Prasetyo <endri.prasetyo@gmail.com> wrote:

From: Endri Prasetyo <endri.prasetyo@gmail.com>
Subject: [MW:2017] Re: WPS
To: materials-welding@googlegroups.com
Date: Thursday, April 23, 2009, 3:15 AM

Parviz,
 
The base material is one of essential variable, if any difference of base metal so the WPS is different too.
 
regards,
Endri

On Wed, Apr 22, 2009 at 7:14 PM, parviz farhadi <parvizfarhadi@gmail.com> wrote:
Dear All,
 
Is it possible to use WPS of ASTM A106 Grade B and its PQR for ASTM A333 Gr 6?
 
Regards,
Parviz





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...