[MW:2027] Re: 2018] qualification of wps

Is there a similar table in Sec IX ?

Thank you

On Thu, Apr 23, 2009 at 2:19 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

Yes, Refer Table 4.1

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari
Sent: Thursday, April 23, 2009 11:13 AM
To: materials-welding@googlegroups.com
Subject: [MW:2018] qualification of wps

 

Hi

according to AWS D1.1 ,a groove weld in 6G position is qualified.now is it possible a single pass fillet weld wps qualified by using   qualifid wps groove weld?(for qualification of groove weld ,impact tests are done )

regard advance

 








--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...