Thursday, April 23, 2009

[MW:2024] Re: WPS

Dear All,
 
Many thanks from your prompt responce. I checked the PQR and it is Impact tested at -50 DEGC. So it is possible to use.
 
Regards,
Parviz

On Thu, Apr 23, 2009 at 11:35 AM, JASPAL SINGH <jaspaldhesi@gmail.com> wrote:

Yes you can use

jaspal singh

On Apr 23, 5:11 am, Dale Jones <dalejones7...@yahoo.com> wrote:
> Parviz, you have not provided enough information to answer this question. What code applies, what testing is required......
>
> Regards,
>
> Dale Jones
>
> --- On Wed, 4/22/09, parviz farhadi <parvizfarh...@gmail.com> wrote:
>
> From: parviz farhadi <parvizfarh...@gmail.com>
> Subject: [MW:2012] WPS
> To: materials-welding@googlegroups.com
> Date: Wednesday, April 22, 2009, 7:14 AM
>
> Dear All,
>  
> Is it possible to use WPS of ASTM A106 Grade B and its PQR for ASTM A333 Gr 6?
>  
> Regards,
> Parviz




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...