Thursday, April 23, 2009

[MW:2020] R: 2004] EN 287 Std

Dear Chinoy,

 

EN 287 is also harmonized with PED 97/23/CEE (European Pressure Equipment Directive), for CE mark on pressure vessels.

It’s the EN equivalent to ASME IX std. Sometimes less flexible (qualified ranges, testing, expiration conditions, ..)

 

Best regards


Alessandro Muroni

CAVE

www.cavesrl.com   

 

Da: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Per conto di Nimesh Chinoy - SigmaWeld
Inviato: mercoledì 22 aprile 2009 7.29
A: materials-welding@googlegroups.com
Oggetto: [MW:2004] EN 287 Std

 

Can anyone please explain to me what is EN287 STD for SS Welding ?

 

Regards,

--
Nimesh S Chinoy



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments: