Dear Prem,

How big is the job ? If not very large than we can make this joint with Induction Brazing at our end.

Regards,

Nimesh S Chinoy

SigmaWeld
Electronics Devices

On Wed, Apr 22, 2009 at 9:00 AM, PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com> wrote:

 
Dear friends

We are trying to braze a SS304L tube # Copper tube with OD=15mm and wall thickness 3mm. The joint is a simple square butt joint. Now we have tried torch brazing with following consumables:
L&T Eutectic 1601 flux + L&T 1601 filler wire.
This is a silver brazing filler wire with @ 40% silver,and balance Cu ,i.e.BAg-4 (EWAC 1601)
However we are not able to achieve torch brazing successfully.
We have even tried with Mathure Silver brazing filler wire and flux, but procedure has failed i.e weak joint.
Actually while brazing the filler material flows towards Copper side and does not flow towards SS304L side resulting in a weak joint and can be easily broken by a blow.
The joint also has to pass helium leak test.

Can anybody suggest suitable brazing procedure and technique.
I have read about furnace brazing but it is not practically possible in our job.
We only have the option of torch brazing.

Regards

Prem Nautiyal
Godrej,Mumbai
Cell: 9820313278

PREM S NAUTIYAL
CELL : 9820313278






--
Nimesh S Chinoy

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...