Wednesday, April 22, 2009

[MW:2003] Ferrite test

Dear All.

Could you pl. advice/ suggest  me about below mention items in ferrite test in stainless steel (Type 304L) overlay and clad restoring welds.

1.  Percent of test per weld seam/length and no. of measurement per test

2.  Method of calculating the average of measurements

 

Best regards,

M. Torkaman


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...