[MW:1985] Re: effect of H on notch strength

Ali,
The top line shows the toughness of the base material without hydrogen embrittlement occurring - toughness increases steadily with increasing temperature.
 
The lower, V-shaped line shows that the effect of hydrogen embrittlement is worst at about 50°C, decreasing rapidly as the temperature increases (and the ability of the hydrogen to diffuse out of the metal increases) and also decreasing at lower temperatures, where reaction rates are much lower and the density of hydrogen increases, hence its volume decreases.
 
Other may wish to add more to this simple approach. Does this help?
 
Regards,
Owen.
----- Original Message -----
Sent: Saturday, April 18, 2009 11:31 AM
Subject: [MW:1980] effect of H on notch strength



hi
can anybody explain about this picture?
rgds.






--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...