[MW:589] Re: Annular bottom plates from API-650 Tanks

Dear Mr. Kannan,
 
I don't think there is any problem in sending the attachment all across as we are doing with our company and to other companies. Since these are soft copies of the docs. which we are circulating we are not breaching the laws of copy rights in any case. These attachments are circulated for sharing the knowledge and not for destructive activities.
 
Regards,
 
S.N.Dave

Kannan.Sundaram@Linde-LE.com wrote:

Dear Friends,

A non- member has posted this message. I am sorry on posting a part para of the API code for better understanding.

I think and suggest to this group, as does yahoogroups, it would be better to avoid even attachments.

I request all others to follow suit and take this seriously as I have now.

Again sorry to all members and moderators for causing to be noticed by someone somewhere.

With regards,
Kannan Sundaram.




"Owen Jenkins" <owen@osjl.co.uk>
Sent by: materials-welding@googlegroups.com
21/02/2008 10:45
Please respond to
materials-welding@googlegroups.com

To
<materials-welding@googlegroups.com>
cc
Subject
[MW:587] Re: Annular bottom plates from API-650 Tanks





Gentlemen,
A word to the wise... You could find yourselves in a lot of trouble for copyright infringement, not only with the API but also Google.
As you are well aware, copyright exists in ALL API material: I advise you NEVER to post illegal copies of copyright material in a public chat room. I realise it was done with the best of intentions to help a colleague in need, but please find another way of communicating the information.
 
I'm posting this advice to help you and others stay out of trouble. We have no idea who is monitoring internet traffic! Unfortunately, today Big Brother undoubtedly IS watching us.
 
I'm in Scotland! These emails are read all around the world.
 
Regards to all,
Owen Jenkins.
 
 
 
----- Original Message -----
From: Kannan.Sundaram@Linde-LE.com
To: materials-welding@googlegroups.com
Sent: Thursday, February 21, 2008 8:58 AM
Subject: [MW:586] Re: Annular bottom plates from API-650 Tanks


I think you are missing the copy of API 650......!


A283 Gr.C comes under group I and the following part of API 650 is self explainatory.


5.5 ANNULAR BOTTOM PLATES

5.5.1 When the bottom shell course is designed using the allowable stress for materials in Group IV, IVA, V, or VI, butt-welded

annular bottom plates shall be used (see 5.1.5.6). When the bottom shell course is of a material in Group IV, IVA, V, or VI and the

maximum product stress (see 5.6.2.1) for the first shell course is less than or equal to 160 MPa (23,200 lbf/in.2) or the maximum

hydrostatic test stress (see 5.6.2.2) for the first shell course is less than or equal to 172 MPa (24,900 lbf/in.2), lap-welded bottom

plates (see 5.1.5.4) may be used in lieu of butt-welded annular bottom plates.


M.4.1 Tanks with diameters exceeding 30 m (100 ft) shall have butt-welded annular bottom plates (see 5.1.5.6).


5.1.5.6 Bottom Annular-Plate Joints

Bottom annular-plate radial joints shall be butt-welded in accordance with 5.1.5.5 and shall have complete penetration and complete

fusion. The backing strip, if used, shall be compatible for welding the annular plates together.


5.1.5.5 Butt-Welded Bottom Joints

Butt-welded bottom plates shall have their parallel edges prepared for butt welding with either square or V grooves. Butt-welds shall

be made using an appropriate weld joint configuration that yields a complete penetration weld. Typical permissible bottom buttwelds

without a backing strip are the same as those shown in Figure 5-1. The use of a backing strip at least 3 mm (1/8 in.) thick tack

welded to the underside of the plate is permitted. Butt-welds using a backing strip are shown in Figure 5-3A. If square grooves are

employed, the root openings shall not be less than 6 mm (1/4 in.). A metal spacer shall be used to maintain the root opening between

the adjoining plate edges unless the Manufacturer submits another method of butt-welding the bottom for the Purchaser's approval.

Three-plate joints in the tank bottom shall be at least 300 mm (12 in.) from each other and from the tank shell.




With regards,
Kannan Sundaram.



"saqib gul" <saqibgul@gmail.com>
Sent by: materials-welding@googlegroups.com
21/02/2008 07:49
Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
[MW:585] Annular bottom plates from API-650 Tanks







Can any body help me out that in which cases we use annular bottom plates for above ground storage tanks? Are there any recommendations in API-650 regarding the use of annular plates? Are the use of annular plates depends on the size of tanks? I am particularly talking about A-283 Gr.C Plates.

 
Regards

Saqib Gul

Design Engineer

Attock Refinery Limited

Pakistan

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...