please note - that it is not necessary for the steel to have CE marking for PED unlike Construction Products - however the steel manufacturer must be 3rd party certified to ISO 9001 - if their certifying (aka  notified) body is not on the EU recognised list then it will be have to be co-certified with a recognised CB
 
Kerrie Christian
Materials & Quality Systems
BlueScope Steel

From: materials-welding@googlegroups.com [materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING) [R.Bathula@ticb.com]
Sent: Tuesday, 14 April 2009 13:20
To: materials-welding@googlegroups.com
Subject: [MW:1936] RE: 969] RE: 947] RE: 865] PED Harmonised Standard for Design

Summary "Comparative Study on Pressure Equipment Standards"

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Agrawal Sunil (Mumbai -Stequ)
Sent: Saturday, July 26, 2008 4:36 PM
To: materials-welding@googlegroups.com
Cc: piping_valves@yahoogroups.com; PED2000@googlegroups.com
Subject: [MW:969] RE: 947] RE: 865] PED Harmonised Standard for Design

 

Friends, recently I attended one seminar on "Awareness training seminar on CE Marking – Pressure equipment directive" conducted by TUV India. I share below my learning:

 

Any std. adopted and published by CEN (European Committee for Standardization – Comite Europeen de normalisation) is known as EN std. (European standard). Incase it is published in "official Journal of the European Union", it is known as "Harmonised Standard". For example, PED 97/23/EC has been published in official Journal of Europa under no. L 181 on 09.07.1997.

 

All std. published in "official Journal of the European Union" can be seen at:

http://eur-lex.europa.eu/JOIndex.do?ihmlang=en

 

You can also search and download the harmonized std from above mentioned site.

 

"BLUE GUIDE" are also available for the interpretation of harmonized stds.

 

If anyone would like to place the product in the European Market, it is mandatory to provide "CE Marking" on it. And to have "CE Mark" one need to follow the appropriate regulation (like PED for Pressure Vessels) and the equipment has to be approved by "Notified Body" if applicable.

 

Hope the above information would be useful to all.

 

Best regards,

 

Sunil S. Agrawal

Static Equipment Dept. (STEQU)

Engineering & Design Tecnimont ICB

101/102, Interface-11, Link Road, Malad (w), Mumbai - 400 064 ( +91.22.6777.7237 * s.agrawal@ticb.com

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Friday, July 18, 2008 2:02 PM
To: materials-welding@googlegroups.com; PED2000@googlegroups.com
Subject: [MW:947] RE: 865] PED Harmonised Standard for Design

 

EN13445 at a glance, interesting presentation

 

-----Original Message-----

From: materials-welding@googlegroups.com

[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula

Raghuram (Mumbai - PIPING)

Sent: Saturday, June 14, 2008 10:22 PM

To: PED2000@googlegroups.com; materials-welding@googlegroups.com

Subject: [MW:865] PED Harmonised Standard for Design

 

Just the below link for more information, interesting one

http://www.unm.fr/en/general/en13445/

 

published hormonised stanadrds for Directive 97/23/EEC can be seen at

http://ec.europa.eu/enterprise/newapproach/standardization/harmstds/refl

ist/equippre.html

and

http://www.newapproach.org/Directives/ProductFamilies.asp?97/23/EC

 

The attached list contains references to harmonised standards for

pressure equipment and harmonised supporting standards for materials

used in manufacturing pressure equipment.

 

The follwoing pretext taken from a CEN link may be helpful

A harmonised standards is a standard considered by the European

Commission as satisfying some of the directives essential safety

requirements.

 

Harmonised standards are covered by three types of European  Standard:-

 

    * Harmonised Product Standards

      These are application codes  that cover the design and manufacture

of Pressure Vessels, Boilers and  Pipework

 

    * Harmonised Support Standards

      Welding, NDT and other  standards that supplement the application

codes.

 

    * Harmonised Material Standards

      A material specified in a  harmonised standard will satisfy the

requirements of the directive in terms of  ductility, toughness and

strength but does not guarantee that the material will  be suitable for

a specific application.

 

 

Each harmonised standard will contain an annex stating  which essential

safety requirements it satisfies.  The advantage of using these

standards is that no additional justification is required that essential

safety  requirements have been met and providing the standards have been

correctly  applied the design of the equipment can not be challenged.

 

Another advantage of using Harmonised Standards is that they  provide an

interpretation of the directive.  For example if a pressure vessel is

to operate below zero the impact tests on the material and welding

procedures  have to be carried out the lowest operating temperature the

vessel will  experience according to ESR 7.5.  This is not current

practice as far as either  PD5500 or ASME VIII is concerned as both

these standards permit, under certain  circumstances, warmer impact test

temperatures.

 

Harmonised Standards are not essential, any appropriate  standard can

used but the satisfaction of essential safety requirements must  proved.

Both PD5500 and ASME VIII have produced annexes stating how and which

essential safety requirements they claim to satisfy, these annexes have

not been  approved by the European commission and therefore neither

standard can claim to  be harmonised.

 

Note PD5500 has nothing to do with the PED, it is simply the  latest

revision of BS5500, it no longer has the status of a British Standard

because it will conflict with BSEN13445.  It is now a  Published

Document rather than a standard,  This will make no difference to it  as

it will continue to be supported as long as its popularity remains

 

The harmonised standard for the qualification of welding personnel is EN

ISO 9606, for operating procedures it is EN ISO 15614. (Note EN ISO

15614  only satisfies the requirements of E.S.R 3.1.2 it does not

satisfy the requirements for welding consumables stated in E.S.R 4)

 

 

-----Original Message-----

From: PED2000@googlegroups.com on behalf of Rajesh

Sent: Sat 14/06/2008 17:37

To: Process Equipment Design

Cc: estamd@graphiteindia.com

Subject: [PED:93] PED Harmonised Standard for Design

 

 

Dear All,

 

I undrstand that Harmonised Standard For pressure vessel design for

PED is being published. BSEN13445. I have some querries.

 

- If this help us in selection of material.

- When this standard is likely to be published.

 

Regrads

 

Rajesh

 

 

 

 

 

 

 

 

 

 

 

 

 

 









NOTICE - This message and any attached files may contain information that is confidential, legally privileged or proprietary. It is intended only for use by the intended recipient. If you are not the intended recipient or the person responsible for delivering the message to the intended recipient, be advised that you have received this message in error. Any dissemination, copying, use or re-transmission of this message or attachment, or the disclosure of any information therein, is strictly forbidden. BlueScope Steel Limited does not represent or guarantee that this message or attachment is free of errors, virus or interference.

If you have received this message in error please notify the sender immediately and delete the message. Any views expressed in this email are not necessarily the views of BlueScope Steel Limited.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...