Weld joint Post weld heating 100°C one hour should be maintained. 
Electric coil heating is preferred to maintain proper temperature.
Based on thickness PWHT to be done. 
To ensure weld quality go for helium leak test. 


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Ch Bilal jovinda <chbilaleng1989@gmail.com>
Sent: Monday, September 15, 2025 8:09:58 PM
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Subject: [MW:35814] Material SA 335 P9 (P No. 5B) Welding with ER 80S-B8 or ER90S-B91
 
Dear Group Members,

We are working with material SA 335 P9 8mm thickness, which has a P number of 5B. For welding this material, we are using consumables ER 80S-B8 or optionally ER90S-B91.

I would like to request members who have experience welding with ER 90S-B91 (closely related to ER90S-B9) to share any necessary precautions or considerations that should be taken during welding.refere below we are taking care,

1.Preheat to 210 degree centigrade minimum.
2. Interpass 300 degree centigrade maximum.
3. What are other recommended?

Best regards,
Bilal Chauhadry,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAOq7hqvpGAzaQ3urEHdwMRqn94bMZ-12BOsL0tkmmkLFLDFFNA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...