Re: [MW:35809] PWHT Requirements for WPS

Mr. Pankaj,
When you are expecting a solution for your problem, Please furnish all the info. at a time and not one after another.
Now u r mentioning about the impact requirement. What is the governing thickness of the welded part and whether 
it is normalised or as rolled /quenched and tempered/fine grained steel. 
CS 



On Wed, 10 Sept 2025 at 16:59, pankaj pachahara <pankajpachahara@gmail.com> wrote:
According to ASME section VIII Div 1, yes we have impact requirement at -20°C. 

On Mon, 8 Sep 2025 at 5:23 PM, 'venkat chikkala' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear,

What is the design code and what about impact requirements of Job.

Regards,
CH V RAMANA 
BVIL

On Monday 8 September, 2025 at 03:39:45 pm IST, pankaj pachahara <pankajpachahara@gmail.com> wrote:


Dear Expert,

I have a WPS for SMAW+SAW process Material SA 516 GR.60/70 with PWHT requirements of 631°C temperature and 450 minutes holding time. 

Now, I have a new project with PWHT requirements of 600±25°C temperature and 3 hours holding time.

Can I use the existing WPS for this new project? What is the acceptable deviation (±) for PWHT requirements?

Looking forward to your guidance.

Best regards,
Pankaj Choudhary 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJF_nWO3GK%2BxVdpQ95N2x5bfsi48-jsgmdCuKLhR_d-Cb4Uynw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/701146338.727314.1757332152427%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJF_nWNBed20VEw1ZKKAo5GV3HGqXkdyv%3DxLNH5RN6oc_e8Hbg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYijjvXL-%2B2o5piYKsRDBw5n-qRpwG919HjVDj_8n9H9QHA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...