Re: [MW:35642] IP Joint

Many thanks Dhana. 

I am new to Aramco project. I will go through the specs. 

Regards 
Saurabh


On Mon, 26 May 2025 at 9:28 PM, Dhanabal Jalachandran <dhanabal.jalachandrann@gmail.com> wrote:
Greetings,

In Saudi Aramco projects, the term "IP" refers to the Initial Production weld for piping joints. As per the requirements of SAEP-324 (Welder Performance Qualification Procedure), every welder must perform a minimum of three (3) Initial Production (IP) welds following the successful completion of their Welder Qualification Test (WQT).

This process ensures that welders not only meet qualification standards in a controlled test environment but also demonstrate their proficiency in actual site conditions before being released for production welding activities.  

Reference - SAEP-324

Best Regards
Dhana

On Mon, May 26, 2025 at 7:27 PM Ganga Prasad <gangaprasad9010@gmail.com> wrote:
Greetings,

I think 'IP' joint means 'incomplete penetration'(partial penetration) joint.




On Mon, May 26, 2025, 7:30 AM 'Eugene Matsko' via Materials & Welding <materials-welding@googlegroups.com> wrote:
In essence, an IP pipe joint is any connection made between pipes that are sized using the IPS or NPS standards, regardless of the specific connection method.

Sent from my iPhone

On May 24, 2025, at 9:48 PM, Saurabh Jain <ensaurabh@gmail.com> wrote:


Hello experts,

I would like to know what is IP joints in piping(31.3)? 

Regards
Saurabh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADr-LL_mAcbc5GDt1TSd_Oip4ns3sqL_mS_AOtP4PyW7a9V9OQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/7BC10B8B-F349-4C33-B40E-20F56C6FB24A%40yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACoqHbO4S8M1DgQCKJAatH4y40G4HY03Ryiwvr6BGxwEBKi8_Q%40mail.gmail.com.



--
Regards
Dhanabal Jalachandran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAPLwtDcC-Li20S1EVK8pZ0AwUmt0WwLdhAr_aSu4bgeNjKLasA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADr-LL9q%2BeJmd3NCTO-BcaK2bOvNFUTbK3JVdNcya3QbZfmSHQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...