Re: [MW:35446] Filler wire for welding off SA182F11 to SA268TP446

Dear Mr. Sujit Kumar,
The details are sourced from Welding handbooks.
I am enclosing a part of it for your records.
rgds,
C S
---------------------------------------------------------------------

On Thu, 20 Feb 2025 at 12:53, sujit kumar <sujitkumar19942@gmail.com> wrote:
Hello Sridhar,

Thank you so much for your response.
May I know the source how you have selected that filler wire for SA182F11 to SA268TP446 welding....if you have any document regarding that could you please share that document. I will be grateful to you.



Thanks and regards
Sujit kumar

On Fri, 14 Feb 2025, 05:51 sridhar cn, <sridharcn305@gmail.com> wrote:
ERNiCr-3 (Inconel 82)  for corrosion resistance or  ERNiCrMo-3 (Inconel 625)  for corrosion resistance 
and extreme environments, or ER309L  for general purpose could be used.
Preheating  & interpass temp. control will help  to minimize the risk of cracking.  PWHT might be necessary 
to relieve stresses and improve the weld properties.
Sridhar.
-------------------------------------------------------------------------------------------------------------------------------------


On Thu, 13 Feb 2025 at 18:41, sujit kumar <sujitkumar19942@gmail.com> wrote:
Hello experts

Greetings for the day.


Kindly please tell me what will be the filler wire for welding of
SA182F11 to SSA268 TP446




Best regards
Sujit kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPKQrt%2Ba3WvcLqQNQA%2BWW6KBw649UUC_Nh2xdcpwHPhzw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYihKtTvsp_3w__4-ZEpwG-YJCumSn%3DABrjWQ-N2%2BD3Q5NQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFonYWOngx4uRU1nAKmYj5bpK6CimrzoTX-ur9wFw5uhPvmyXA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYiigwv6Uf5VhYHXbbBdv_aWsf5%3DUFk7LB%2B9WcqbiFjjyzA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .