Re: [MW:35428] Re: ASME Sec. VIII Div. 1 - MDR form U1 / U1A

The points to be included in the "Notes" section of Form U-1A depend on the type of vessel (e.g., cryogenic, NACE, or lethal service) and the material used (SS, Duplex, or Carbon Steel). Below are the common points to consider:

Common Points to Include in U-1A Notes:

1. Radiographic Examination (RT)

Percentage of the vessel subjected to RT (e.g., "Shell and heads 100% RT per UW-11(a)").

Acceptance criteria (e.g., "RT per ASME Section VIII, Div. 1, UW-51").


2. Post Weld Heat Treatment (PWHT)

If applied, mention the temperature and holding time (e.g., "PWHT at 1150°F for 1 hour per UCS-56").

If exempted, state the exemption clause (e.g., "PWHT not required per UCS-56(d)").

3. Impact Testing

If required, reference the applicable impact test exemption rules (e.g., "Impact tested per UG-84" or "Exempted per UCS-66").

4. Material Certification

If material traceability applies, note it (e.g., "All materials comply with ASME Section II, Part A and B").

Mention any dual-certified materials (e.g., SA-516 Gr. 70 / SA-515 Gr. 70).

5. Special Service Conditions (if applicable)

If designed for cyclic service, reference U-2.

6. Design Code & Special Considerations

Mention any Code Cases used.

Any Finite Element Analysis (FEA) carried out for specific weld joints.

Type of Bolt, Stud, and Washer used.

Best regards,
Deerendra
+91-9112146005

On Sun, 9 Feb, 2025, 19:49 israr, <ahmedisrar.nm@gmail.com> wrote:
Dear Team,
Could anybody tell what specific points to write in Notes of form U-1A?
Our AI always change the points every time.


On Friday, February 11, 2011 at 10:38:54 AM UTC+5:30 Prasad wrote:
Dear experts & ASME Authorized Inspectors,


Our company have ASME certificate of authorization for ASME U stamp
with scop covering
manufacturing activities at shop & field sites controlled by our
company.
We have constructed a pressure vessel at field site owened by our
customer.
Now we have to prepare MDR in U1 form.
My question is againest name & address of manufacturer whether we have
to put field site address or address of our company as apeared on
certificate of authorization.

Please share your experience & views on above.

Thanking you.

Prasad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ee319b7c-bfad-49a4-b12d-66970c6653f8n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9GAi7uQeke%2B_qSue_NOQEGq%2BhKQbmKm9c_33yPMSdMbdg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...