Re: [MW:35369] Pipe 304L(P8) – Pipe 304L(P8)

Yes . E/ER 308L is having beter corrosion resistance  but strength reduces marginally. You can also try E/ER 308LM

On Mon, 18 Nov 2024 at 17:39, Marco Nunes <marcovsky82@gmail.com> wrote:
Can  anyone provide some assistance in the issue identified below:


The details are as follows:

 
Details

Parent material Pipe 304L(P8) – Pipe 304L(P8)
Inservice temperature range – 35-85 °C
Operating Pressure – 0.4 -0.5 MPaG
Process Type – Process Condensate.
Carbonic acid – there may be the presence of carbonic acid as indicated by CGCL.
 

Approved Process

WPS# P8-P8 AR - Filler material ER308L- F6 filler metal
 

Quality Issue

ER308H rods were used instead of ER308L on two locations of the 304L piping.
 

Technical Advice Request

The client indicated that the use of the ER308H Filler Wire instead of the ER308L has a higher risk of intergranular corrosion and corrosion related issues.  
 

Please advise on the short term or long-term quality effects on the integrity of the welded joints where the ER308H filler wire were utilized.

 

Thanking you in advance.

Mark Nunes

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHXTn13_GqEVg7xyKfzH26pgfOGr8us4_2HTsfih1tPZn-vFwQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oh5yaenUFNs4TGO8OCh7ix39xJHMJwiSzAbuNRQpmbAsg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...