Skip to main content

Re: [MW:35322] Pipe Insert Sleeve - How to ensure after hydrotest No Water

Dear Mr. Aravindh,

Thank you for your reply.
How did you have ensured there is no water between sleeve insert and pipe?
This insert used not to get corrosion inside weld joint area. While performing trail we have prove that no hydrotested water entered in very tiny gap. 

Thank you, 
Regards, 
S.SENTHILKUMAR


On Tuesday 12 November, 2024 at 05:47:07 am GMT+3, s.aravindh ram <aravindhram22@gmail.com> wrote:


Dear sir,
I have worked in oman,  used this  high pressure line we will apply gloves insert this bevel joint after welding welding complete hydrotest will be conducted as per designed pressure,
After that testing we will the spool for erection.
Thankyou
Aravindh


On Fri, 8 Nov 2024, 7:09 pm 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear All,

Please see below picture Pipe Insert Sleeve in my site taking trial and completed hydrotest as proto type. Now how to ensure there is no water between Pipeline and insert sleeve. 
Any body have experienced in this please give feedback. 
Thanks 
Inline image


Thank you, 
Regards, 
S.SENTHILKUMAR

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/115108384.237400.1731070617477%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGH_84AoxZnJcJez4FnCTxduc984PsFksajgiq6kmHPVen2wTg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...