Hi, As per ASME B31.3, Table A1-M,  -46 Deg Celsius is the minimum temperature applicable without impact test.



But Please consider the below note description also before concluding. It is better to do an impact test below -29 degree celsius.




On Wed, Apr 24, 2024 at 4:29 PM 'vinit vani' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Dear All,

Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX

Material  to be used used during Fabrication - SA 333Gr6 (P No.1 Gr. 1) To SA 350-LF2 (P No.1 Gr. 2)

Production Thickness range-5.54mm(Minimum)-9.53mm(Maximum)
PWHT – Nil
MDMT-= -45 Deg Cel.
Kindly give your valuable suggestions for applicability of PQR impact requirement for above details.
Pl.reply with code clause.
Thanks & Regards
Vinit
India

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/670487658.2039399.1713956840743%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JNqER%2BNMC-5qaM8d%3DZ8vgJc84Wo%2Bc5OMHw%3DCp_5aaSAEQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...