Sunday, April 21, 2024

Re: [MW:34915] Filler wire

Dear saleem,

Please refer attached image,

Regards,
Shahil 

On Sun, Apr 21, 2024, 10:39 saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear Sir

     Could you share, where it's mentioned 

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs


On Sun, 21 Apr 2024 at 9:04 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
E71T-1C  is Charpy Impact tested at -20degC
E71T-1CJ is Charpy impact tested at -40degC.

AWS Classification for FCAW is only a supplementary requirement applicable only when Impact test is required.

If charpy impact test is not required then you can use E71T-1C in place of E71T-1CJ

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Sunday, 21 April, 2024 at 11:02:44 am IST, saleem manhappulath <saleemm9526@gmail.com> wrote:


Dear Experts 


     We have wps it's mentioned filler wire E71T-1CJ, but in the market available only E71T-1C. What is the difference between two filler wire and can we use E71T-1C instead of 1CJ

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmvvSvr_KHHb0thJJ2gotwiCMYU3TNsAwPcHgT_8f%2BDoLg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1947962007.973816.1713679243043%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmujkxSODsnhZp%2B5Xs-GCeL%3DM8_%2BLS1fpQ1nHY8SEsHaew%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-VSHE2Jui-rsN%3D_k-MqbU6hVc7nBCWuN_yfiK%3Da9XHOg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...