Re: [MW:34907] Thickness range in WPS for Fillet

Both of u correct. As per sec IX u r correct and As per Sec8 ( referring code) he is also. While choosing the WPS, to be careful whether it address all requirements of Reference code. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Apr 18, 2024 at 1:33 PM Shivasankar A <shivasankar2593@gmail.com> wrote:
Thank you Mr. Srinivas. I got what I was looking for, through your response .

On Wed, Apr 17, 2024 at 7:35 PM srinivas rao <engr.srini@gmail.com> wrote:
Due to the PWHT requirement  for joints over 38mm - refer to UCS-56

Thanks & Regards
Srinivas Rao

On Wed, Apr 17, 2024 at 2:14 PM Shivasankar A <shivasankar2593@gmail.com> wrote:
Dear team,

can anyone clarify my issue.

During the preparation of WPS & PQR of SA 516 GR 70 to SA 516 GR 70 - 10mm Plate Groove weld, my AI (Authorised Inspector) was insisted me to put the Thickness range for fillet weld as 38mm maximum in both WPS & PQR. 

I am unable to understand this. Because as per ASME Section IX Table QW451.4 - All groove weld tests can qualify "All fillet sizes on all base metal thicknesses and all diameters" So according to my understanding it should be unlimited but why my AI insisting me to put as 38 mm max..

Pls Clarify.

Regards,
Shivasankar A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b568812e-6355-43a5-8574-0fc6a039a5acn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/V9ooFlYXrL4/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHdRSONy-gzpzZOWK%2B8nE70%3Dj6UvQpV5Dq8DYnb7Cr%3DjZDgppA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG%2BrNO9MawYXdJQ4Rb-q09DVu8DZHB3xW2mLT%2BJq-%2BNPM5HTgQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMCCCy2fHPsJVvj9VL-sxmDm%3D5-Ttyn7-jHB1OSROQt_g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...