Re: [MW:34861] WPS for overlay (QW 403.20)

Thank you!
I don't understand how QW403-20 is different from QW403-11?

What does it mean for QW 403.20 to determine the chemical composition of the weld metal overlay specified in the WPS? Can you please explain clearly here? Is it possible to determine the chemical composition of the weld overlay in PQR after the overlay is completed? What is the method to determine it?

Thank you for your contribution!

Best ragards!
....................................
DƯƠNG VINH QUANG - WELDING ENGINEER
● Welding Team - Central Engineering - NSRP
Phone: +84 (0) 964 801 295




On Wed, 10 Apr 2024 at 14:13, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
This clause is pertaining to substrate Base material (P.No.) over which weld overlay is Done.

Normally the Client specification or the mandate code will specify the chemistry of the overlay and at what depth from the Fusion line.

An example of Refinery code giving chemistry requirement in API RP-582 below.



Hope now you can read and understand.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Wednesday, 10 April, 2024 at 10:47:15 am IST, Dương Vinh Quang <duongvinhquanga13@gmail.com> wrote:


Dear experts,

I'm writing WPS for overlay following ASME IX, but I have a concern about section QW 403.20 " If the chemical composition of the weld metal overlay is specified in the WPS, a change in the P-Number listed in Table QW/QB-422 to another P-Number or unlisted base metal, or a change in Group Number for P-No. 10 or P-No. 11 base metals.
If the chemical composition of the weld metal overlay is not specified in the WPS, qualification on P-No. 5A or any lower P-Number base metal also qualifies for weld metal overlay on all lower P-Number base metals".

I hope that you can help me to explain about this paragraph. If possible, please give me a specifc example. Thank you all!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/40c92c78-d955-4db9-bb71-14be4a366225n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1538150546.4493684.1712732061871%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdNLKhCQqgXCxm10qgysXuYjmx%3DpGjf_wapcfkk6FuwTqk0EA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...