Required Consumable formula 
W= A x e x L x 1/E
 Where, 
W= Required  quantity / Filler metal ( grams)
A = Cross section of Area ( cm2)
e= Density of material 
L= length of the weld in cm 
E= Deposition efficiency
 


A= ((rxt)+(t-f)2xtan(θ/2))/100

Where,
r = root
t = thickness
F= Foot face 


Thanks and regards, 

   


Masna Uday Kumar

Ph:9063983052

masnaudayk4@gmail.com

 



On Mon, 8 Apr 2024 at 12:42 PM, SMM <sohilmehta@gmail.com> wrote:
Dear Experts, 

How to calculate consumables required in SMAW/MIG/TIG process

The welding in running meter are as below 
1800m  of IS2062 steel 8mm thick
630m of SS316L stainless steel 6mm thick
3500m of lining inside shell 2mm thick 

Are there any other dimensions required for calculations

Thank you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/52f6ad61-e224-41af-ab74-4ffd1a6d897fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOOs2YZX7MazgSsnyCHOU49cadjwyhLc4HbHYh_R4L2b99OFDg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...