Re: [MW:34849] Welder qualification on WPS/PQR qualified as per ISO 15614-1.

Better to go with ISO


On Sat, 6 Apr 2024, 3:45 pm Ritesh Kumar Singh, <riteshsiwan770@gmail.com> wrote:
Dear experts.

I have a query regarding welder qualification details as following. 
I have a WPS and PQR qualified as per ISO standard. 
can I qualify welders as per ASME sec 9 with that WPS or I have to follow EN ISO 9606-1 ?
Kindly advise. 

Thanks & Regards
Ritesh kr. Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-id5ypCk6_d6AnnJwGP4mLZ%2BeDxLs-s8OWZE6%2BARF8NZg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEabyKm1EQC35WFpaV5purcMFMfk9nyvQ4j-aPHxBWe9EYtzSg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...