Tuesday, April 30, 2024

[MW:34929] ASME SEC VIII Div1- UG-36 & UG-42 Nozzles RF pad requirements & mulitiple Nozzles opening

Dear all,
Kindly refer to the attached images of the 
2 instrument air vessels.
one vessel 6" nozzles with reinforcement pad and other one same 6" nozzles without RF pad. Top head diameter, design pressure, head thickness , nozzle to head weld is internal portrusion with back side welding also same

From UG-36 above 10mm thickness only 2.3/8" ID nozzles can fabricate with out reinforcement pad.

Queries:
1. 6" nozzles required RF pad or not? With details explain 
2. 6" nozzles in-between 2" nozzles with maintain 500mm centre to distance - min distance requirements.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYwuPbWBjMbyfZcbS4De_tJ23EVbs4KSNcy%3Du8q8p7Wi2w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...