Thursday, August 31, 2023

Re: [MW:34521] I request for your expert advice

Is it an option to only use a spot GTAW weld for fixture of the thread
Or seal it with Loctite
To prevent shrinkage during welding, very low heat input process like laser welding can be an option


Regards,

Weld-Tech BV
Jurgen Prinsen (MSc/IWE)



Van: "Balasubramanian M" <bala.smi@gmail.com>
Aan: "materials-welding" <materials-welding@googlegroups.com>
Cc: "Balasubramanian M" <bala.smi@gmail.com>
Verzonden: Donderdag 31 augustus 2023 09:36:43
Onderwerp: [MW:34520] I request for your expert advice

Dear Experts,
I am writing this for you to give me some advice/suggestions.

We are facing a severe issue in welding the Body-end connector joint in our small-size (0.75" 800#) 2-piece Ball Valves Lever Operated SW ends (MOC 316 with PTFE seat ring). Since our client wants us to seal weld the Body-End connector joint, after assembly and final testing prior to despatch.

We find that after welding, in TIG, the valve becomes very difficult to operate.
I request the experts in this group to suggest a suitable method to weld the joint.

Best Regards.
M.Balasubramanian

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD5c4ZzPm9sap4GGRRTiPnU_4Emzm4jtAjZu7%2BvybuvfbKKRNg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...