u might used 5356 or 5556,
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Tue, Aug 22, 2023 at 9:30āÆAM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
Dear ExpertsALUMINIUM 6082 -T6 - 32mm , 20 mm , 16 mm plates32mm ,-32mm- Butt joint20 mm-20 mm-Butt joint16 mm - 16 mm -Butt jointAbove plates are jointed through butt joints .Welding Process - GMAWGas - ArgonFiller wire - ER4043Due to job part length , there is distortion at the vicinity of butt welds. So Cold straightening operation was carried out on Press. The weld/HAZ cracking is observed immediately the press load is commencedPl. suggest suitable action for Welding/cold straighteningThanksVishwas - IWE--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/597ef31f-53c7-4c81-9924-cbbdd688c49an%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePu3mUEPdaDkyrntUvhFzVN1FkFqCKdND3EjnDqUXCC8g%40mail.gmail.com.
Comments