Wednesday, August 16, 2023

Re: [MW:34490] Welding materials SA-240 310s (P.no8) to SA-213 T11 (P.no4)

what is the thickness. 
If Thickness is less than 13mm, Preheat T11 side and weld T11 + ASS with ER NiCr3
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Aug 16, 2023 at 8:27 AM 'Ahmed Osman' via Materials & Welding <materials-welding@googlegroups.com> wrote:
* if PWHT is needed for 213 T11  ... cladding technique will be used ( 1st clad P4 with ERNiCr-3 then finalize PWHT ) (2nd weld with P8 with same electrode )
* If PWHT not needed for 213 T11 and
   - service temp. less 315c     -- use 309L
   - service temp. more 315C  -- go with ERNiCr-3

best regards
Ahmed Osman



On Monday, August 14, 2023 at 02:26:15 p.m. GMT+3, Mohamed Elsayed <m.sayed0994@gmail.com> wrote:


Hello dears
I'm going to weld SA-240 310s (P.no8) to SA-213 T11 (P.no4), but I don't know what is the proper electrod or filler metal to weld this material, so help me please

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKujbmu2ZYjN8UsS-ko2PZu0YT1EUHFBV1JPHM8ZdNvRP65E_Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/440702323.980444.1692078418046%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePEPeoBVx6GXApP8tod769z5h2v4N2t_gMEti_qRF9P4Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...