Monday, August 14, 2023

Re: [MW:34486] ER70S-2 and ER70S-6 (GTAW Process) - A number

it means  need not test weldmetal again while doing PQR. 

On Mon, Aug 14, 2023, 9:32 AM MW <raghurambathula@gmail.com> wrote:
just to update
ASME Boiler & Pressure Vessel Code 2023 Edition Significant changes include:
-Added an optional supplemental "A" designator to indicate that an ER70S-6A electrode or R70S-6A rod has met the chemical composition requirements of A-No. 1 (SFA-5.18/SFA-5.18M).
-Added optional supplemental designators to indicate ranges of shielding gases for which an electrode meets the requirements for classification, including any optional, supplemental designators. This resolves major issues previously associated with determining the A-No. for these filler metals.

On Wednesday, 10 July 2019 at 08:48:11 UTC+5:30 dili...@gmail.com wrote:
ER70S-6 chemical composition does not allow A-No allocation. 

Στις Πέμ, 6 Ιουν 2019, 14:40 ο χρήστης Revdiwala Darshan <darshanm...@gmail.com> έγραψε:
Please refer QW-404.12 (f) for code restriction.

Regards,
Darshan

On Mon, 3 Jun 2019, 6:26 pm Kannayeram Gnanapandithan, <kgpan...@gmail.com> wrote:
Code doesn't restrict but u will not get it in cut to length. Hardness will also increase due to more Mn, Si. It is better to add ER 70S3

On Mon, 3 Jun 2019 7:48 pm K K, <kara...@gmail.com> wrote:
Dear All,

My PQR is qualified with ER70S-2.

Can I use ( Mention) ER70S-6 in WPS.

Regards
Kiran


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4955a6fe-a91e-4b08-8f15-5aaa363df01cn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMERRAgCM63OVeadMEY05XjnNYezLwdtGSK9kea%3DPvdtQ%40mail.gmail.com.

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...