Dear Mr. Ali,
We can support for calibration block and inspection by PAUT, as we have aluminum block available with us. 
If you require support for the same, you can write us on info@ndtsolutions.co.in.
Regards,
Vishal Gherwada
ASNT LEVEL III -UT
ISO 9712 LEVELV III - UT & PAUT
                      On Wednesday, 2 August, 2023 at 08:37:55 am IST, 'Ali Bhatti' via Materials & Welding <materials-welding@googlegroups.com> wrote:                  
                  Dear experts 
We have to weld 30" dia and 25 mm thickness of aluminum materials .
suggest me alternative of RT, PAUT , joints are confined area 
1. Due to space RT is difficult , and for PAUT additional material not available to prepare test pieces / calibration blocks 
Best Regards 
-- 
--- 
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/D4B0725F-CC26-4936-88F3-C9CBDC52D645%40yahoo.com.
Comments