for impact test requirements at what temperature? - material-wise reference as we should follow B31.3 table A-1,
Figure 323.2.2A Minimum Temperatures Without Impact Testing for Carbon Steel Materials(refer Table A-1 to find out the impact test requirements as per materials and which graph want to refer)
Table 323.3.5 Minimum Required Charpy V-Notch Impact Values
Table 323.3.4 Charpy Impact Test Temperature Reduction
Table K323.3.1 Impact Testing Requirements
Table A-1 Basic Allowable Stresses in Tension for Metals

The highest heat input reduction in yield strength and low toughness (grain growth) is closely related to hardness, thus heat input calculation is required.  

On Monday, 31 July 2023 at 06:18:43 UTC+3 Uma sankar Sankar wrote:
Good morning experts
      

          In WPS ,from where we need to get Impact test qualified thickness ranges (min - max). what are dimensions of Test coupon,and how can we decide the impact test temperature?why Heat input should be calculated,when ever impact test required in wps,is hardness required for ever joint ? please give ur best in the point of Saudi Aramco projects.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/82931196-9d1f-4fc3-8ab1-809c694ecaden%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...