Re: [MW:34053] Re: FILLER WIRE FOR SS 304 TO SS321

When welding SS304 to SS321 materials, the recommended filler metal is usually an austenitic stainless steel filler metal, such as AWS A5.9 ER321 or ER347.

AWS A5.9 ER321 is a titanium-stabilized austenitic stainless steel filler metal designed for welding 321 and 347 stainless steels. It has good oxidation and corrosion resistance and can be used for welding in high-temperature applications.

AWS A5.9 ER347 is a niobium-stabilized austenitic stainless steel filler metal designed for welding 321 and 347 stainless steels. It has excellent high-temperature strength and oxidation resistance, making it suitable for welding in severe service conditions.

The selection of the filler metal will depend on the specific application and the welding process being used. It is recommended to consult the applicable code or standard and a qualified welding engineer or metallurgist for specific guidance on selecting the appropriate filler metal for your application.


On Tue, Jan 17, 2023 at 7:30 AM Student <nabeel233@gmail.com> wrote:
Check AWS D1.6 for guidance 

On Wednesday, November 23, 2022 at 12:18:43 PM UTC+3 sujit kumar wrote:
Dear experts

what will be the filler wire for SS304 TO SS321 MATERIAL






Best Regards
Sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/466ab234-1197-4993-9d00-99d8412c3bb6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFhOWxZif_Eqo4Wnn65nvBEU2qVj5kadOA4JhRSQT-NVxOnK2Q%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...