Skip to main content

Re: [MW:34052] Consumable Selection

Hi
Has any body procedure for pipeline pigging?

Thanks
M. Hussein

On Thu, Mar 2, 2023 at 5:11 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Use 316Ti, for 6CrNiMoTi 17122. and for 13CrMo 4-5 either NiCr3 or 309 ( based on service Temp)
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Feb 22, 2023 at 9:12 AM Anand Elankumaran <email2uranand@gmail.com> wrote:
Dear Experts,

Could you Please advise if the below consumable selection is correct or not.

WPS Requirements as per BS EN 15609 & 15614

Material

Size

Process(Est. Weld thk)

Material Grouping  as per PD CR ISO 15608

Suitable Consumable

Remarks

GTAW

SMAW

1.4571EN  X 6 CrNiMoTi 17 122 to
1.4571EN  X 6 CrNiMoTi 17 122

22.3 X 2.77

GTAW (2.77)

8.1

ER 316L-17

--

(Exaton 316/316L-17)

1.4571EN  X 6 CrNiMoTi 17 122 to
1.4571EN  X 6 CrNiMoTi 17 122

168.3 X 10.97

GTAW + SMAW (4 + 6.97)

8.1

ER 316L-17

E 316L-17

(Exaton 316/316L-17)

1.7335EN, 13CrMo4-5 to
1.4571EN X 6 CrNiMoTi 17 122

33.4 X 3.38

GTAW (3.38)

8.1 - 5.1

ER NiCrMo-3

--

 

 


--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChwvFgCTrAHGN4Jp62zbaUGPfo%3D2YjVi7Vn8y44q9eufcQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNFMDnEksFYoUNmh%2BM%2Ba4LkFJpkWjhxWELKMX3WZ5%2B0WQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVihNFadeA%2BFLxx5PphQuQMAFfv5rPUYrRN%3Dt%3DUNWbDv%2Bj3w%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...