Weld the joint as per attached configuration as a single vee joint using alloy filler wire/electrode such as ER/E NiCrMo3 for the complete joint.
Thanks & Regards
J.Gerald Jayakumar
On Friday, 23 December, 2022 at 04:35:28 pm IST, atul jha <atulkrjha21@gmail.com> wrote:
Dear sir
-- I Have to establish a PQR as per below detail :-
Material 1 : SA 516 gr 70 overlay of 3 mm by NiCrmo-3 ( done at vendor works).
Material 2 : A182 Gr F 44 UNS S 31254.
Code of construction ; B31.3.
Pwht : none
I have to weld this joint in our plant as per attach figure.
QUERY: can a PQR with P1 to P8 by nicrmo-3 will serve the purpose OR I have to establish a PQR P1 ( cladded by nicrmo-3 ) to P8 welded by NicrMO-3 . I want to go with 1 st case
Does change in welding process also affect the above choice .
Kindly note that these vessel are for ARAMCO.
Kindly explain and guide me accordingly.
Regards
Atul jha
B.E in welding Technology.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC1tTUKXF5UizBMZH-tJTz7TDJtRaijzggwtJ4gCfbQxHGYP7Q%40mail.gmail.com.
Comments