Gentleman,

SA234 WP22 is for 2.25Cr-1Mo steel

where as P91 is modified 9Cr-1Mo steel with additions of Nb and V which provides higher creep strength at applicable higher temperatures and which differentiates from P9 steel (9Cr-1M0).

See below snap shot

Inline image

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 20 December, 2022 at 08:49:29 am IST, mithlesh kumar <mithleshmech47@gmail.com> wrote:



Sir please read WP22 instead of P91
On Monday, December 19, 2022 at 3:01:56 PM UTC+5:30 kannayeram gnanapandithan wrote:
P/T 91 is CrMov steel
It should have Vanadium  and it is a precipitation hardening elements.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Dec 19, 2022 at 8:43 AM Vishwas Keskar Welding Manager WELDING <vvkes...@gmail.com> wrote:
What is the % Vanadium in that MTC ?
It is trace elements not a deliberate addition for Gr 22  unlike Gr 91 where it it MUST in Gr 91 

Regards

Vishwas IWE
International Welding Engineer 


On Saturday, December 17, 2022 at 8:47:13 PM UTC+5:30 mithlesh kumar wrote:
Kindly read WP22 instead of P91
On Saturday, December 17, 2022 at 8:15:23 PM UTC+5:30 mithlesh kumar wrote:
Dear team,

I have observed vanadium in heat analysis of p91 MTC  , but as per code vanadium is not showing in chemical composition table. Suggest is it acceptable or not if acceptable code reference please.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/21151b29-5972-4606-930c-0fc03e313713n%40googlegroups.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...