Monday, December 19, 2022

Re: [MW:33832] Re: Vanadium composition showing in p91

P/T 91 is CrMov steel
It should have Vanadium  and it is a precipitation hardening elements.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Dec 19, 2022 at 8:43 AM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
What is the % Vanadium in that MTC ?
It is trace elements not a deliberate addition for Gr 22  unlike Gr 91 where it it MUST in Gr 91 

Regards

Vishwas IWE
International Welding Engineer 


On Saturday, December 17, 2022 at 8:47:13 PM UTC+5:30 mithlesh kumar wrote:
Kindly read WP22 instead of P91
On Saturday, December 17, 2022 at 8:15:23 PM UTC+5:30 mithlesh kumar wrote:
Dear team,

I have observed vanadium in heat analysis of p91 MTC  , but as per code vanadium is not showing in chemical composition table. Suggest is it acceptable or not if acceptable code reference please.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1f2331d9-3cb1-437c-adc3-ba7b8be6f9f8n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOLphF-d1neVrQ0QBG_jSODTk__pOsX5NpNspk_HX_Qgw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...