Dear Mr. Ponnni

If the Filler Metals are provides as per ASME SEC II C then the Test Certificate shall be as per ASME SEC II C requirement of SFA-5.01M/SFA-5.01. No other tests are required as per ASME while receiving the consumables.

Generally for Corrosion Resistant Materials, Clients specify PMI testing of materials at least for a single item in a lot. This is based on the client requirements. 

Thanks & Regards
Sham Shahabuddin
On Tue, Nov 29, 2022, 1:25 PM Ponnikumar <k.ponni1994@gmail.com> wrote:
Dear gentlemen,
My client inspector told me to do button weld test on plate for filler wire 309L . The dimension are follow as asme sec II c then need to do PMI verification 

My query is any requirements by code for filler wire button test for all filler and electrode and why it required ? 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYw73OyFYLq4yTHUB2cVqbuaDCCunxc73%2BaU0kJZurJd%2Bw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyAb6NT7zuC4m6ng%3DivendMf68wXs9s2TZOW9UMcEaYE-Wq3Q%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...