Monday, December 12, 2022

Re: [MW:33813] Request for information to Make BSEN PQR

For european materials, ref ISO/TR-20172, For ASME--ISO/TR-20173 & For japanese materials -ISO/TR-20174

16Mo3----group no 1.1, and 13 Cr Mo 4-5-- group no-5.1

On Sun, Dec 11, 2022, 7:40 AM Anand Elankumaran <email2uranand@gmail.com> wrote:
Dear Experts,

Please advise the below information for making the PWPS & PQR as per BS EN 15609 & 15614,

WPS Requirements as per BS EN 15609 & 15614
Material Material Grouping  as per
PD CR ISO 15608
Suitable Consumable Preheat requirement PWHT Requirement
GTAW SMAW
1.5415EN, 16Mo3           
1.7335EN, 13CrMo4-5           

--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChzJOvd175bZh6y-RBZ_cHuooiGrLOwRJkZNEg%3DE5dyZ1w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOTvMgjVjpJ-tKgLzmxd8Kvi%2BYe4hUpMhk3AemkB694jQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...