Skip to main content

Re: [MW:33808] Duplex, super duplex stainless steel repair

Hi S32750 is a super duplex grade. Repair welding is always more tricky than original welding. Irrespective of the issues, as 90% of the weld contains defects causing rejection, it would be advisable to remove the previous weld by machining and reweld with matching filler. As the base metal is S32750 (according to description) ER-2594 filler should be used. Welding heat input & welding parameters control should be exactly same as the Procedure Qualification.
DSS/SDSS are always used in extremely corrosive environments, hence due control of welding parameters and following the rules of fabricating DSS/SDSS would be advisable.
Aramco has extensive guidelines on welding DSS/SDSS. You may follow those or ask for that information as needed.

RT is difficult to perform on branch welds.However may be possible for larger dia welds.

Thanks. 
P.Goswami, P.Eng, IWE.

On Friday, December 9, 2022 at 10:14:01 a.m. IST, Ganesh Muthurajan <qceng.mg@gmail.com> wrote:


Hi Mr. Ragu

The material grade is S32750.
And we found leakage in service, 

We will have random RT 90% are rejected and moreover PMI confirm the material in duplex not super duplex. 

after the root cause analysis we found corrosion on weld. Not in pipe and fittings.

The WPS used in production having more heat input compare then root pass. 






On Thu, Dec 8, 2022, 10:59 AM Raghuram Bathula <raghurambathula@gmail.com> wrote:
Dear Ganesh
what grade?, what type of failures (in NDE or in service?), any root cause analysis done.
Knowing the root cause and extent of damage is very important before attending repairs.

if you are considering these are as closure joints, then only Volumetric examination is permitted, otherwise check feasibility for in service testing

On Thu, 8 Dec 2022 at 13:22, Ganesh Muthurajan <qceng.mg@gmail.com> wrote:
Good morning sir, 

Now i working with duplex and super duplex , RO plant.

How to do the repairs in this material, for example we found two segment in 10 mm  in 14 inch pipe. 

Can we do partial repair, or fully cutout and reweld.  Any code reference advice to do full cutout, or partial.

Second case this plant was handed over to the Clint, during commissioning we found leakage, not only the butt joint, even in the branch connection, 

Aramco advise to do 100 %rt butt joint and branch.

Branch we can't do RT, placing a film is deficult.  What to do in this. 

Please advise me your experience and international, Aramco code reference.


Thank you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM0EmFJPK-9Z8w9M%3D0wje6%2Bd%2BH%2Bn_7-SZmhy7R2ksEv_SYEB3w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnMUK_U0EbNLjNjNceka_wcTxq9WvWEd_hLa%3D77ot7hfQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM0EmFJHUBkuGuyhVirJO_kOZO-xQ4rz9Xgybwy27yUEUofUSQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...