Depends on code and specifications as I remember in B31.3 it is  5T( wall thickness of pipe*5).


On Thu, 1 Dec 2022, 8:48 AM Yunsok Bang <stevebang87@gmail.com> wrote:
Hello.


This link will help your question.

In my work place follow the BS code. The 4t(nominal pipe thickness).

Have a good day.

On Wed, Nov 30, 2022 at 2:42 PM Mahmood Al-Hinai <hyna4444@gmail.com> wrote:
Experts,

What is the requirement for the distace between branch weld and pipe seem weld. 
Is the condition in attached photo accepted or not?
Pls advise

Thanks
Mahmood

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEuX%2Bdk%2BkMiraG4-1YmWuRhwrgCLczaPZYgvpUGVyEoQV00jmA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACrdFNRtMBnkY57Kag58OoxgBbj%3Dy-jreWi5i8xncCYRCYtWMA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-i9D_%2B%3DUPdnBwi%2BxR3zgnhdAzT7XjPt%3D8wxj9sB4C-JhA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...