Friday, December 23, 2022

[MW:33847] Technical quary for Electrode E8010 using instead of E7010

Dear Sir.
   Any have TQ for above subject please share me. My site using E8010 .but Site document mention E7070.so I need TQ for Using E8010.
Thank you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw8uFh0UP%2BruTnOPTF7LHjMUWEuzSzeuavfcq%3DOUEHgFTg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...