Dear Sir 

At @ 900-940 Deg C , the Carbon will react  with Ti /Nb/Cb to form its carbides . This   results into no Carbon or very less Carbon will be available  to form Chromium Carbide which is  detrimental to corrosion resistance.

Thanks and regards

Vishwas - IWE
International Welding Engineer 
 

On Thursday, December 22, 2022 at 8:53:38 AM UTC+5:30 Prakash Hegde wrote:
Hi! Friends
Why some of the client spec ask for
Stabilizing treatment (At lower temperature than solution annealing i.e. about 900C) of already solution annealed plate but not Welded SS components

Especially  304H,347,321

Regards
Hegde

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4869cfea-8374-4bcf-9154-d224480f611bn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...