Saturday, December 17, 2022

[MW:33823] Re: FILLER WIRE FOR HASTELLOY

ERNIMO10

On Monday, October 31, 2022 at 8:42:28 AM UTC+5:30 sujit kumar wrote:
Dear expert 
What is the filler wire for below mentioned mention Material

1. FILLER WIRE FOR HASTELLOY B TO HASTELLOY B  BASE MATERIAL WELDING

2.FILLER WIRE FOR DUPLEX TO DUPLEX BASE MATERIAL WELDING

3. FILLER WIRE FOR ENCONEL 602 TO SS 316 BASE MATERIAL WELDING 


Best regards
Sujit kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3645bf50-b018-47a2-a61d-2ea2aa44d043n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...