Re: [MW:33621] Re: Auto Tig for SS 310 with Ar+H2 gas

u can use Ar +He

On Tue, Oct 25, 2022, 9:21 AM Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:
Single V.. 60 deg included angle.. 0mm root face with 1-1.5mm root gap

On Fri, 21 Oct 2022, 09:23 Vishwas Keskar Welding Manager WELDING, <vvkeskar123@gmail.com> wrote:
What is  joint configuration and thickness?


On Friday, October 21, 2022 at 8:42:52 AM UTC+5:30 Hrushikesh Sangamnerkar wrote:
Dear experts,

Query is can we weld Auto Tig (with Filler) for gas combination of Ar+Hydrogen? Pl provide technical literature to support the question,if available at your end.

Currently facing an issue of LOP with Argon gas only..

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fd385e70-f227-46b5-bebc-3254f318e711n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2pgGOo8z%2BkW80AQ2KFUZbbCWpsdcrMREWG66VY%2BNrttiw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNoT2KwXQRX%2B2zRAXPP0bEdAU0cAycfrNaFC3SNN2q4Ng%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...