Refer UG-10 it says recertification by Vessel or part manufacturer and it allows to certificate holder recertify the material as per current edition, without NCR. Also additionally you can refer ASME Section II Mandatory Appendix II for more details and example.

On Friday, October 7, 2022 at 1:01:57 PM UTC+5:30 Saurabh Joshi wrote:
Dear All ,

     We have to manufacture a Heat ex-changer Code of construction ASME 2021(Code stamp required for the Equipment) . Raw material for plates & pipes are manufactured As per ASME 2019 . MTCs are available as per ASME 2019 and Original marking is still available on materials how can i re-certify the material and use it for the equipment which has the code of construction ASME 2021 .


Regards
Saurabh Joshi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3bda27ee-07d5-41d9-8a1d-2a7063314b2en%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...