Yes it can be done

On Tue, 11 Oct 2022, 11:50 williams p wilson, <williamswilsonp@gmail.com> wrote:
Dear Experts,

Please guide, RT can be replaced with PAUT for a vessel constructed with ASME Section VIII Div.1, MOC : SA 516 Gr.70, 70 / 80 mm Thickness.

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ5hNvmec_a_qxOBGp66-DVsdUR7mT3WHOvS-%3DKX_dq4vg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp9M7vMpBfB3YM6h0G4ZiJTDqMbTSPBP91LhR652Q2Pw%2BA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...