[MW:33587] Black dots on sdss welding

Dear Team,

Can you please explain about the black dots appears on SDSS GTAW Weld bead( ER 2594 )  with document backup for the causes 


Regards,

M.Kumar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADTvyj%2B9Ti77s60HeABOGGgrcOeok0BG2nwCqMQQ8zrDqdyGyw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS