Dear Experts,

Could you please suggest suitable FCAW welding electrode for the below specifications,

MOC : SA 516 Gr.70 + N , 70 mm Thickness
PWHT :  610 ° C x 300 minutes minimum
Impact Test after HT @ -29° C, 32 J for 1 specimen, 48 J Avg. for 3 specimens. 

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ6pfMSGDbpH5rVktdwS6O0qYrHFk6FC_GBrz-aH408OsQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...