Re: [MW:33614] Auto Tig for SS 310 with Ar+H2 gas

Use the below chart.

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Friday, 21 October, 2022 at 07:12:48 am GMT+4, Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:


Dear experts,

Query is can we weld Auto Tig (with Filler) for gas combination of Ar+Hydrogen? Pl provide technical literature to support the question,if available at your end.

Currently facing an issue of LOP with Argon gas only..

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2piyXRMx4A4tXavwmxnn-6dO4PkfAEZzw%2B4Cwd15h4TmA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...