Hot-dip galvanized pipe is to make the molten metal react with the iron matrix to produce 
an alloy layer, so that the matrix and the coating are combined.  

1. The chemical combination varies as per the grade. 
    for example, (Gr. 33, 37, 40, 50, 80 type as per ASTM A 653) has 

    Carbon (C)              0.20 to 0.25 (max)
    Manganese (Mn)    1.35 (max)
    Sulphur (S)             0.04 (max)
    Phosphorous (P)    0.04 (max)

    UTS                        45 to 82 Ksi.  (min. as per the grades)
    Yield                       33 to 80 Ksi.  (min. .........                   )
  % of El.           12 to 20    (min, .........           )

2. Grade CSA has  Mn 0.60 max. other elements more or less the same.

Sridhar.
---------------------------------------------------------------------------------------

On Thursday, 6 October, 2022 at 08:47:49 am IST, Ezenwa Victor <victorvery@gmail.com> wrote:


Dear Team 

What's the Chemical composition of a Galvanized Steel pipe 1" and 1 1/2".

Thanks 

Engr Ezenwa Victor 
SON Nigeria


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BSLriOMdo3wcsPb%3DEDt8oiF6D5OYMYSFGEF8K7vFyDwvaJV9Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...