Tuesday, October 25, 2022

Re: [MW:33621] Limitation of FCAW process

if it is solid wire, ur spec ok because  different metal transfer. For FCAW  to my knowledge,  no restrictions 

On Tue, Oct 25, 2022, 9:21 AM pradip kumar Sil <pradipsil@gmail.com> wrote:
Dear all,

Our contract document is restricted for FCAW process upto 25 mm thickness and design temperature not less than minus 10 degree centrigrad for all pipe welding.

Any specific reason for the  limitation of particular process.

Thanks in advance.
Pradip

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DKz1LWV0ofaEnFpSnWDXoaAo_utePdx_MKfbg%2B7CzmEQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePN7NARoPqkawK88dU4L9gNmb2Ls%2BABiScWE5d1-Q_0wA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...